What pigment, paint and coating dispersants does LigninCorp supply?
LigninCorp supplies pigment, paint and coating dispersants for pigment wetting, particle stabilization, slurry stability, color consistency, grinding support, anti-agglomeration and water-based formulation systems. Key product families include Dispersant NNO, Dispersant MF, sodium lignosulfonate, sodium alkyl naphthalene sulfonate wetting agent and wetting-dispersing blends. Buyers can use this page to match coating formulation requirements with product families, prepare TDS, SDS/MSDS and COA requests, and send formulation conditions for grade recommendation.
Pigment and Coating Applications Covered
Pigment Slurry Dispersion
Particle dispersion, slurry stability and reduced agglomeration
Paint and Coating Stability
Color consistency, suspension stability and formulation support
Powder and Pigment Wetting
Faster wetting, improved mix-in and reduced floating or clumping
Ink and Color Paste Processing
Grinding support, particle distribution and color paste consistency
Industrial Suspension Control
Grade comparison using solids, pH, particle type, viscosity and stability target
Procurement and Technical Documentation
TDS, SDS/MSDS, COA, packing, samples and grade comparison
Which products fit each pigment or coating requirement?
How are pigment dispersants added, and at what dosage?
The lignosulfonate dye and pigment dispersant (GAC-DP) typically starts at 2–8% of the dye or pigment solids, with 3–5% for first trials; fine, high-surface-area pigments need the upper end. The dispersant is dissolved in the water phase before the pigment is added and ground. Ranges are typical starting points from our technical data sheets unless marked as published practice; the final dose is set by laboratory or plant trial.
| Product | Typical starting dosage | Notes |
|---|---|---|
| Lignosulfonate dye and pigment dispersant (GAC-DP) | 2–8% of dye or pigment solids; start at 3–5% | Dye powder, pigment grinding and ink formulation. |
| Calcium lignosulfonate, dispersant grade | 0.1–1.0% of material weight | Pigment and filler systems; bench test required. |
| Wetting and dispersing agent blend | 0.2–2.0% on solids or formulation | Pigment and ceramic slurries; adjust with viscosity and pH. |
| Wetting agent OT / AOT | 0.05–0.5% (coatings and inks); 0.1–1.0% (pigment systems) | Strong wetting at low dose; control foam. |
How to add it
- Dissolve first: dissolve the dispersant in the water phase and, for lignosulfonates, bring the pH to about 8–10 (published practice) before adding pigment.
- Add pigment under stirring: add the pigment gradually to the stirred liquid to make a smooth premix, then grind in the bead or ball mill.
- Find the optimum: run a dose curve and choose the dose at the lowest stable viscosity; more dispersant past that point brings no benefit.
- Standardize: record the dose for each pigment type and keep it constant between lots for consistent colour strength.
Points to check
Calcium and other dissolved salts can thicken lignosulfonate pigment slurries, so water quality matters. Lignosulfonates are brown, which limits their use in white and pale shades.
Trial checklist
- Particle size by laser diffraction or Hegman gauge
- Viscosity at each dose and after storage
- Settling and colour strength against the current dispersant
- Foam during grinding
What details help LigninCorp recommend a coating dispersant?
- Application type, such as pigment slurry, paint, coating, ink, color paste, grinding system or water-based suspension.
- Target function, including wetting, dispersion, viscosity control, color consistency, anti-settling or storage stability.
- Pigment type, filler type, resin or binder system, water phase, pH and solids content.
- Grinding process, target particle size, viscosity range, compatibility limits and dosage target.
- Required documents such as TDS, SDS/MSDS, COA, specification sheet or sample request.
- Packaging, order quantity, destination country and shipment timeline.
Pigment Paint and Coating Dispersant FAQs
Which dispersants are used for pigment dispersion?
Dispersant NNO, dispersant MF, sodium lignosulfonate and sodium alkyl naphthalene sulfonate wetting agents may be reviewed for pigment dispersion depending on pigment type, pH, carrier system, solids content and stability target.
Can lignosulfonate support paints and coatings?
Selected lignosulfonate grades can support pigment wetting, particle dispersion and slurry stability in suitable water-based systems. Compatibility with resin, binder, salt level and pH should be confirmed before final approval.
When should buyers review a wetting agent?
Wetting agents are useful when powders or pigments are difficult to wet, disperse or incorporate into a water-based system. They can be reviewed together with dispersants when both fast wetting and storage stability are required.
What documents are useful before sample testing?
Buyers commonly request TDS, SDS/MSDS, COA, packing information and application notes before lab evaluation. LigninCorp can prepare document support according to the selected dispersant or wetting agent family.
What dosage of lignosulfonate dispersant is used for pigments?
The lignosulfonate dye and pigment dispersant typically starts at 2–8% of the pigment solids, with 3–5% for first trials. The best dose is the one that gives the lowest stable viscosity and the target particle size.